含埋藏裂纹缺陷长输管线的安全评定及剩余寿命计算
详细信息 本馆镜像全文    |  推荐本文 | | 获取馆网全文
摘要
采用GB/T19624-2004标准,对长输管线中的埋藏裂纹缺陷进行安全评定,在评定的过程中选取了4种壁厚不同的X80管线进行常规评定,计算出了断裂比、载荷比并绘制出了失效评定图。采用Pairs公式对一段含缺陷在役管线进行剩余寿命计算,为管线的维修、检测提供了一定的理论依据。
Based on GB/T19624-2004,safety assessment for hidden crack defects of long-distance pipeline lack was carried out,four kinds of X80 pipelines with different thickness were selected for general assessment,the fracture ratio and load ratio were calculated,and the failure assessment diagram was drawn out.The remaining life of a pipeline in service with defects was calculated by using Pairs formula,which can provide a theoretical basis for repair and testing of the pipeline.
引文
[1]沈士明.在役压力管道安全评定研究的现状与发展[J].中国机械工程,2007,8(3):101-104.
    [2]ASME Nuclear Power Plants Components Code Nc-3658,ASME SectionIII[G].
    [3]王文和.含缺陷压力管道安全评定方法研究的现状与发展[J].管道技术与设备,2007(2):1-3.
    [4]余建星,詹强,吴海欣.穿越管道的疲劳失稳风险评估方法的研究[J].地震工程与工程振动,2001,21(2):58-63.
    [5]周昌玉,张艳丽,李强,等.在役压力管道含缺陷结构腐蚀疲劳剩余寿命预测的随机分析[J].压力容器,2002,19(2):14-17.
    [6]GB/T19624-2004在用含缺陷压力容器安全评定[S].
    [7]李培宁.国际压力容器缺陷工程评定技术进展[J].压力容器,1991,8(2):3-6,.
    [8]罗金恒,赵新伟,白真权,等.输油管道腐蚀剩余寿命的预测[J].石油机械,2000,25(2):17-19.
    [9]钟群鹏.我国压力容器安全评定技术的现状和发展[J].中国机械工程,2005,8(5):95-100.
    [10]任志平.大中型穿越河流输油管道的风险评估[D].大庆:大庆石油学院,2004.
    [11]刘曦.含焊接缺陷结构的疲劳可靠性评定及其专家系统[D].南京:南京化工学院,1993,19(1):66-72.

版权所有:© 2023 中国地质图书馆 中国地质调查局地学文献中心