Hexagonal RuB1.1 were synthesized using ruthenium and boron powders as raw materials during ball milling process.
Orthorhombic RuB2 were synthesized under high pressure (5 GPa) and high temperature (1000 °C) conditions.
Hexagonal Ru2B3 have been synthesized under 5 GPa and 1200 °C.