摘要
通过长时间的生产和维护实践,对马钢2250 mm热轧卷取机各种类型的堆钢进行跟踪分析,总结出堆钢产生的原因,并制定相应的措施,有效降低了堆钢发生的几率。
Through long term production and maintenance practice, we tracked and analyzed various types of strip heaping accidents at the 2250 mm strip down coiler of Masteel,concluded the causes of the problem and drew up corresponding measures, which has effectively reduced the risk of strip heaping.