摘要
某铁矿石嵌布粒度较细,矿石比较难磨,对其进行精准取样,开展选矿试验研究。试验结果表明,TFe品位24.01%的铁块矿,在-400目90.8%的磨矿细度下,经过"预选-三段磨矿-五段磁选"流程选别,可获得精矿TFe品位55.66%、回收率55.07%的选别指标,选矿比4.209倍。
A certain iron ore embedded granularity is relatively fine, and the ore is relatively difficult to grind. Accurate sampling of iron ore bodies in iron mines is carried out, and mineral processing experiments are carried out.The test results show that TFe grade of 24.01% iron ore,in grinding, granularity-0.037 mm accounts for 90.8%, under such conditions,by implementing the separation process of "pre-selection ore-three sections of grinding ore-five segments of magnetic separation", the iron concentrate TFe grade of 55.66% and recovery rate of 55.07% can be obtained.Mineral dressing ratio is 4.209.
引文
[1] 邱俊,吕宪俊,陈平,等.铁矿选矿技术[M].北京:化工出版社,2009.
[2] 陈雯.贫细杂难选铁矿石选矿技术进展[J].金属矿山,2010,407(05):55-59//80.
[3] 罗良飞,陈雯,严小虎,等.低品位复杂难选铁矿选矿技术进展及研究方向[J].矿冶工程,2010(30):48-53.
[4] 马淮湘.超贫磁铁矿选矿技术新进展与思考[J].现代矿业,2011 (04):33-34//42.
[5] 吴蓬,吕宪俊,邱俊.超贫微细粒难选磁铁矿的磁选试验研究[J].矿物岩石,2015,35(01):7-12.
[6] 邱俊,吕宪俊,李全京,等.山东汶上低品位铁矿石的矿物学特征及磁选实验研究[J].矿物岩石,2009,29(02):12-17.
[7] 陈晓鸣,李广涛,张宗华.四川攀西地区某难选铁矿的工艺矿物学及选矿试验[J].矿业研究与开发,2008,28(04):34-37//63.
[8] 刘桂卿,赵运欢,邱俊,等.某低品位铁矿石的选矿工艺研究[J].现代矿业,2010,499(11):14-16.
[9] 吕宪俊,孙丽君,杜飞飞.某低品位铁矿石的矿物学特性与选矿试验研究[J].金属矿山,2010,409(07):75-77.
[10] 李朝晖,徐麟,郭秀平.某铁矿细粒难选铁矿石磁选工艺研究[J].现代矿业,2014(03):131-133.
[11] 邱俊,王周全,吴蓬,等.甘肃某铁矿石工艺矿物学研究[J].金属矿山,2016,479(05):95-98.
[12] 阎赞,王露,王想,等.某超贫磁铁矿干式预选-湿式磁选试验研究[J].矿产综合利用,2017(05):27-30//36.